MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ PVDF 11010/0000 Polyvinylidene Fluoride
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: 3M™ Dyneon™ PVDF 11010/0000 is a copolymer of VF2 and HFP (hexafluoropropylene). Recommended for flared tubing, it combines excellent chemical resistance, and dimensional stability with a moderate degree of flexibility. PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and oil and gas industry, PVDF is also gaining recognition in automotive, building, electronics, food processing, and pharmaceutical equipment and battery applications.
  • Good flexibility and mechanical strength in extruded tubing
  • Flareability of extruded tubing
  • Good chemical resistance to acids, bases, alcohols, ect
  • Meets requirements of Factory Mutual Standard FM 4910
  • NSF 61 Certification

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption <= 0.040 %<= 0.040 %24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound  2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psi50mm/min; ASTM D638
Tensile Strength, Yield 27.0 MPa3920 psi50mm/min; ASTM D638
Elongation at Break 400 %400 %50mm/min; ASTM D638
Flexural Strength 37.0 MPa5370 psi2mm/min; ASTM D790
Flexural Modulus 0.900 GPa131 ksi2mm/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °F
Vicat Softening Point 150 °C302 °F1 kg load; ISO 306
Flammability, UL94 V-0V-0
Oxygen Index >= 44 %
@Thickness 3.00 mm
>= 44 %
@Thickness 0.118 in
Sheet; ASTM D2863
 
Descriptive Properties
FormGranules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride
BASF Ultradur® B 6550 L PBT
BASF Ultradur® B 6550 LN PBT

PDYNE068 / 34876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.