System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
BASF Ultradur® B 6550 LN PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.30
g/cc
0.0470
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
0.25 %
0.25 %
23°C; 50% RH
Water Absorption at Saturation
0.40 %
0.40 %
DIN 53495/1L
Viscosity Test
160
cm³/g
1.60
dl/g
Viscosity number; ISO 1628
Linear Mold Shrinkage, Flow
0.019
cm/cm
0.019
in/in
Sheet; ISO 294
Linear Mold Shrinkage, Transverse
0.022
cm/cm
0.022
in/in
Sheet; ISO 294
Melt Flow
11.7
g/10 min
@Load 2.16 kg,
Temperature 250 °C
11.7
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
56.0
MPa
8120
psi
5 mm/min; ISO 527-2
Tensile Strength, Yield
56.0
MPa
8120
psi
50 mm/min; ISO 527-2
Elongation at Break
>= 3.5 %
>= 3.5 %
50mm/min; ISO 527-2
Elongation at Yield
3.5 %
3.5 %
50 mm/min; ISO 527-2
>= 50 %
>= 50 %
50 mm/min; ISO 527-2
Modulus of Elasticity
2.60
GPa
377
ksi
ISO 527-2
Flexural Strength
76.0
MPa
11000
psi
ISO 178
Charpy Impact Unnotched
22.0
J/cm²
@Temperature -30.0 °C
105
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.600
J/cm²
@Temperature 23.0 °C
2.86
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
5.00e+15
ohm-cm
5.00e+15
ohm-cm
IEC 93
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 93
Dielectric Constant
3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 250
3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 250
Dielectric Strength
39.0
kV/mm
991
kV/in
IEC 243/1
Dissipation Factor
0.0019
@Frequency 100 Hz
0.0019
@Frequency 100 Hz
IEC 250
0.0219
@Frequency 1e+6 Hz
0.0219
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index
475
V
475
V
Test solution A; IEC 112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
9.00
-
15.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
5.00
-
8.33
µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Melting Point
220
-
225
°C
428
-
437
°F
DSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi)
135
°C
275
°F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi)
55.0
°C
131
°F
ISO 75-2
Decomposition Temperature
>=
290
°C
>=
554
°F
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Diameter 0.400 mm
HB
@Diameter 0.0157 in
Ignition Temperature
350
°C
662
°F
ASTM D1929
Processing Properties
Metric
English
Comments
Melt Temperature
250
-
270
°C
482
-
518
°F
Pipe extrusion
250
-
270
°C
482
-
518
°F
Semi-finished extrusion
260
°C
500
°F
for shrinkage test
260
-
270
°C
500
-
518
°F
Injection-molding
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Injection molding
60.0
°C
140
°F
for shrinkage test
Descriptive Properties
Color
Natural
Commercial Status
Europe
Primary Processing Technique
Coating and Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultradur® B 6550 L PBT
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
BASF Ultradur® B 6550 PBT
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride
PBASG0092 / 131726
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.