MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mafic Direct Basalt Roving 17 µm Diameter
Categories: Ceramic; Other Engineering Material; Composite Fibers

Material Notes: Continuous direct draw filaments produced from basalt rock used for reinforcement of thermoplastics and thermosets.

Sizing available (sizing agent = silane) for polypropylene, epoxy, vinyl ester, polyester, polyurethane, nylon, or PET/PBT. Also available unsized with deionized water only as the sizing agent.

Information provided by Mafic Basalt

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.63 g/cc0.0950 lb/in³DIN 65569
Moisture Absorption <= 0.10 %<= 0.10 %
Loss On Ignition >= 0.40 %>= 0.40 %Varies with Sizing
Filament Diameter 9.0 µm9.0 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3000 MPa435000 psiASTM D2343
Elongation at Break 3.5 %3.5 %
Tensile Modulus 86.0 - 90.0 GPa12500 - 13100 ksiASTM D2343
Tenacity >= 0.600 N/tex>= 6.80 g/denier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mafic Direct Basalt Roving 19 µm Diameter
Specialty Materials SCS-6 Silicon Carbide Monofilament
Mafic Direct Basalt Roving 13 µm Diameter
Mafic Assembled Basalt Roving 3500 to 4800 Tex
Kuraray Vectran® UM 1500/300 LCP Fiber

EMAFC006f / 230563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.