MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Specialty Materials SCS-6 Silicon Carbide Monofilament
Categories: Ceramic; Carbide; Other Engineering Material; Composite Fibers

Material Notes: High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced titanium, aluminum and ceramic composites are high in strength and stiffness, lightweight, and maintain their properties at high temperatures. Tests have proven that high fiber strength is maintained up to 1200°C. SiC fibers do not react with typical matrix alloys.

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.08 g/cc0.111 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3900 MPa566000 psi
Elongation at Yield 0.90 %0.90 %
Modulus of Elasticity 380 GPa55100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 ohm-cm0.0100 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.10 µm/m-°C
@Temperature 20.0 °C
2.28 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.710 J/g-°C0.170 BTU/lb-°F
Thermal Conductivity 18.0 W/m-K125 BTU-in/hr-ft²-°F3D PTR method
Sublimation Temperature 2300 - 2500 °C4170 - 4530 °F
Maximum Service Temperature, Air 1400 °C2550 °F
 
Descriptive Properties
Cross SectionRound
Diameter142 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mafic Direct Basalt Roving 17 µm Diameter
Mafic Direct Basalt Roving 19 µm Diameter
3M Techical Ceramics MYCROSINT® CD Boron Nitride
3M Nextel™ 550 Industrial Ceramic Fiber
CeramTec V 679 Alumina, 99.7%

ESPEC01 / 6056

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.