MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® FEP 6100 Fluoropolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: DuPont™ Teflon® FEP 6100 fluoropolymer resin is a melt-processable fluoropolymer resin specifically designed for high-speed extrusion of thin coatings on small-gauge wires for twisted-pair constructions.

As shown in Table 1, this resin provides the electrical and mechanical properties needed for low voltage applications. In addition, Teflon® FEP 6100 has a higher melt flow rate than most other fluoropolymer resins. This permits higher extrusion speeds and easier processing, making Teflon® FEP 6100 a cost-effective alternative for producing thin-wall extrusions.

Teflon® FEP 6100 possesses a balance of processing and performance properties, which makes it an excellent choice for many applications. Like all Teflon® fluoropolymer resins, Teflon® FEP 6100 offers an excellent combination of properties:

  • low flammability
  • exceptional dielectric properties
  • heat resistance
  • toughness
  • flexibility
  • low coefficient of friction
  • nonstick characteristics
  • negligible moisture absorption
  • chemical inertness
  • performance at temperature extremes
  • weather resistance

Applications

Teflon® FEP 6100 is especially suitable for use in insulating data and telecommunications cables with excellent fire performance and physical properties as well as outstanding electrical performance. Cables insulated with Teflon® FEP 6100 have met the requirements of the NFPA 90A ‘Standard for the Installation of Air-conditioning and Ventilating Systems’. To meet these requirements cables are tested using the NFPA 262 Standard Method of Test for Flame Travel and Smoke of Wires and Cables. This standard test method is used to qualify cables for installation in plenum spaces under the provisions of NFPA 90A. Teflon® FEP 6100 complies with ASTM 2116.

Teflon® FEP 6100 is not recommended as a jacket material or as a heavy-walled insulation in constructions where significant thermal cycling may raisestress-cracking concerns.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.14 g/cc2.14 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %24 hours; ASTM D570
Melt Flow 30 g/10 min30 g/10 minASTM D2116
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength, Ultimate 20.0 MPa2900 psiASTM D1457
Elongation at Break 300 %300 %ASTM D1457
Flexural Modulus 0.520 GPa75.4 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Coefficient of Friction 0.080 - 0.300.080 - 0.30ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1e+6 Hz
2.03
@Frequency 1e+6 Hz
ASTM D2520
Dielectric Strength 53.0 kV/mm1350 kV/in100 micrometers film; ASTM D149
Dissipation Factor 0.00057
@Frequency 1e+6 Hz
0.00057
@Frequency 1e+6 Hz
ASTM D2520
Arc Resistance >= 300 sec>= 300 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 264 °C507 °FASTM D3418
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 360 - 385 °C680 - 725 °FCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Detergent Resist. on grit-blasted aluminum, Hours600
Detergent Resistance on aluminum, Hours744
Detergent Resistance on grit-blasted steel, Hours480
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm5-80 E3
Heat of Combustion J/g5100ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours>744
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance20Years unaffected in Florida Exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® FEP 5100 Fluoropolymer Resin
Chemours Teflon® FEP CX5010 Fluoropolymer Resin
Chemours Teflon® FEP FR5020 Fluoropolymer Resin
Chemours Teflon® FEP CJ-95 Fluoropolymer Resin
Chemours Teflon® FEP FR5030 Fluoropolymer Resin

PDU9257 / 33352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.