MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTOWAX® AV 5012 Ethylene Vinylacetate Copolymer Wax
Categories: Polymer

Material Notes: VESTOWAX is synthetic waxes produced essentially by two different processes, the Ziegler polymerization and the Fischer-Tropsch process. The Ziegler polymerization of ethylene synthesizes polyethylene waxes with different densities and molecular weights depending on the preparation conditions. The Fischer Tropsch process yields straight chain products possessing low viscosity in the melt and having molecular weights between 500 and 1000g/mol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc
@Temperature 23.0 °C
0.0343 lb/in³
@Temperature 73.4 °F
DIN 53 479
Viscosity 400 - 600 cP
@Temperature 140 °C
400 - 600 cP
@Temperature 284 °F
DIN 52 007/1
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 12 - 1412 - 14mg KOH/g; DGF M-IV 2
 
Mechanical PropertiesMetricEnglishComments
Penetration 3.0 - 6.03.0 - 6.0number in mm, 10-1; DGF M-III 9b
 
Thermal PropertiesMetricEnglishComments
Dropping Point 99.0 - 104 °C210 - 219 °FDGF M-III 3
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Innospec VISCOWAX® 453 Oxidised EVA-Wax
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)

PHUMB454 / 81456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.