MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Innospec VISCOWAX® 453 Oxidised EVA-Wax
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: CAS Number: 104912 - 80 - 3

VISCOWAX® 453 – high quality oxidised ethylene vinyl-acetate copolymer wax.

Application:

  • Plastic processing
    • Pigment processing and additive concentrates Hotmelts
      • Viscosity adjustment and improvement of flexibility and tack
      Applications as water-based Emulsions:
      • Printing inks and Lacquers
        • Low solvent and water-based printing inks and lacquers
        • As antisettling agent in metallic lacquers
      • Leather processing
        • Additive for synthetic resin dispersion used for finishing, fulling and smoothing of upper leather
      • Floor polishes
        • Antislip additive

      Information provided by Innospec Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 - 0.960 g/cc0.0340 - 0.0347 lb/in³DIN EN ISO 1183, C
Viscosity 150 - 250 cP
@Temperature 140 °C
150 - 250 cP
@Temperature 284 °F
DGF M-III 8
Molecular Weight 1500 g/mol1500 g/molGPC
Vinyl Acetate Content 15 - 18 %15 - 18 %FTIR
 
Mechanical PropertiesMetricEnglishComments
Penetration <= 10<= 10[10-1 mm], Needle; DGF M-III 9b
 
Thermal PropertiesMetricEnglishComments
Solidus 83.0 - 94.0 °C181 - 201 °FDGF M-III 4a
Dropping Point 90.0 - 100 °C194 - 212 °FDGF M-III 3
 
Descriptive Properties
AppearanceOff White
Saponification value>80 mg KOH/gDGF M-IV 2
Type of deliveryFine grain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Innospec VISCOWAX® 334 Granules EVA-Wax
Honeywell A-C® 405T EVA copolymer
Honeywell A-C® 400A EVA copolymer
Evonik VESTOWAX® AV 5012 Ethylene Vinylacetate Copolymer Wax
ICO Polymers ICOTEX™ 520-5004 1000 Micron EVA Powder

PINOS033 / 183476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.