MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low moisture sensitivity, toughness, and dimensional stability.

Data provided by Dow Chemical.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM Data
Water Absorption 0.17 %0.17 %
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120
Tensile Strength, Ultimate 48.3 MPa7010 psiASTM Data
Tensile Strength, Yield 57.9 MPa8400 psiASTM Data
Elongation at Break 120 %120 %ASTM Data
Elongation at Yield 6.5 %6.5 %ISO Data
Tensile Modulus 1.59 GPa231 ksiASTM Data
Izod Impact, Notched 5.87 J/cm11.0 ft-lb/inASTM Data
Charpy Impact Unnotched NBNBISO Data
 NBNBISO Data, Low Temp
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO Data, Low Temp
 6.70 J/cm²31.9 ft-lb/in²ISO Data
Instrumented Impact Total Energy  67.8 J
@Temperature -30.0 °C
50.0 ft-lb
@Temperature -22.0 °F
 67.8 J
@Temperature 23.0 °C
50.0 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 77.0 µm/m-°C
@Temperature 20.0 °C
42.8 µin/in-°F
@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FUnannealed; ASTM Data
 110 °C230 °FAnnealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C186 °FUnannealed; 104°C (219°F) annealed; ASTM Data
Vicat Softening Point 117 °C243 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
Covestro Baydur® GS PUR Polyurethane
Dow Isoplast® 202 Polyurethane (PUR-RT), Impact Modified
Isoflon PUR Polyurethane

PDW060 / 34291

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.