MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AlphaGary Evoprene™ COGEE 638 SEBS Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.
Processing: compatible with polypropylene and polystyrene for co-molding or co-extrusion

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccISO 2781
Viscosity Measurement 9.0
@Temperature 150 °C
9.0
@Temperature 302 °F
Kg/cm2; Macklow-Smith extrusion rheometer
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ISO 868
Tensile Strength 5.80 MPa841 psiISO 37
Elongation at Break 398 %398 %ISO 37
100% Modulus 2.50 MPa
@Strain 100 %
363 psi
@Strain 100 %
ISO 37
300% Modulus 4.30 MPa
@Strain 300 %
624 psi
@Strain 300 %
ISO 37
Adhesive Bond Strength 1.77 MPa257 psi
Tear Strength 48.0 kN/m274 pliISO 34-B
Abrasion 165165mm3; DIN 53516
Compression Set  50 %
@Temperature 23.0 °C,
Time 259000 sec
50 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 87 %
@Temperature 100 °C,
Time 79200 sec
87 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 88 %
@Temperature 70.0 °C,
Time 79200 sec
88 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
Ozone ResistanceNo Cracks100 pphm / 200 hrs / 20% strain, ISO1431

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ COGEE 631 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ COGEE 637 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 6087 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 614 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 940 SEBS Thermoplastic Elastomer

PGARY9749 / 140542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.