MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Victrex APTIV™ 1300-100G Black Polyetheretherketone (PEEK) Polymer Film
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: APTIV™ 1300 film is the black version of unfilled semi-crystalline films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications offering an alternative option to the APTIV 1000 natural product.

APTIV 1300 film has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products and low moisture absorption in a film format. Inherently halogen free and providing ease of processing makes APTIV films a technology enabler.

    Applications:

  • Acoustic speaker diaphragms and voice coils
  • Composites
  • Aerospace insulation
  • Pressure sensitive tapes
  • Washers in high speed motors
  • Washers in mobile phone hinges
  • Flexible surface heaters
  • Pressure sensor membranes
  • Proven temperature resistance to use of lead free solders

    Features
  • High heat resistance
  • Excellent tribological properties
  • Broad chemical resistance
  • Low moisture absorption
  • High strength and toughness
  • Stable, excellent electrical insulation properties
  • Good flammability performance without use of flame retardant additives
  • Inherently halogen free
  • Radiation resistance
  • Low smoke and toxic gas emission
  • Excellent hydrolysis resistance
  • Excellent acoustic properties
  • High purity
  • Light weight
  • Recyclable
  • Easy to process - can be laminated to other materials, thermoformed, metallized, coated, printed, stamped and die cut, welded, heat sealed, and coated.

Information Provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc
@Temperature 23.0 °C
1.30 g/cc
@Temperature 73.4 °F
ISO 1183
Thickness 50.0 microns1.97 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 150 %>= 150 %ISO 527
Film Elongation at Break, TD >= 150 %>= 150 %ISO 527
Tensile Modulus 2.30 GPa334 ksiTD; ISO 527
 2.40 GPa348 ksiMD; ISO 527
Film Tensile Strength at Break, MD 120 MPa17400 psiISO 527
Film Tensile Strength at Break, TD 110 MPa16000 psiISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm
@Temperature 23.0 °C
4.00e+16 ohm-cm
@Temperature 73.4 °F
100V; ASTM D257
Dielectric Strength 190 kV/mm4830 kV/inMD, 6.25mm (0.25in) electrode; ASTM D149
 190 kV/mm4830 kV/inTD, 6.25mm (0.25in) electrode; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD  <= 2.0 %
@Temperature 200 °C
<= 2.0 %
@Temperature 392 °F
TM-VX-84
 <= 2.0 %
@Temperature 200 °C
<= 2.0 %
@Temperature 392 °F
TM-VX-84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Victrex APTIV™ 1300-050G Black Polyetheretherketone (PEEK) Polymer Film
Evonik VESTAKEEP® Film 0FH80 PEEK
Evonik VESTAKEEP® Film 0FH90 PEEK
Evonik VESTAKEEP® Film 0FH81 PEEK
Covestro MAKROFOL® UV 503 9-2 060004 Polycarbonate Film

PVICTA84a / 171869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.