APTIV™ 1300 film is the black version of unfilled semi-crystalline films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications offering an alternative option to the APTIV 1000 natural product. APTIV 1300 film has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products and low moisture absorption in a film format. Inherently halogen free and providing ease of processing makes APTIV films a technology enabler. Applications:- Acoustic speaker diaphragms and voice coils
- Composites
- Aerospace insulation
- Pressure sensitive tapes
- Washers in high speed motors
- Washers in mobile phone hinges
- Flexible surface heaters
- Pressure sensor membranes
- Proven temperature resistance to use of lead free solders
Features- High heat resistance
- Excellent tribological properties
- Broad chemical resistance
- Low moisture absorption
- High strength and toughness
- Stable, excellent electrical insulation properties
- Good flammability performance without use of flame retardant additives
- Inherently halogen free
- Radiation resistance
- Low smoke and toxic gas emission
- Excellent hydrolysis resistance
- Excellent acoustic properties
- High purity
- Light weight
- Recyclable
- Easy to process - can be laminated to other materials, thermoformed, metallized, coated, printed, stamped and die cut, welded, heat sealed, and coated.
Information Provided by Victrex. |
Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |