MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features & Benefits:
  • High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applications
  • Low loss tangent - Excellent high frequency performance
  • Thermally stable low profile and reverse treated copper foil - Lower insertion loss and excellent thermal stability of traces
  • Advanced filler system - Improved drillability and extended tools compared to alumina-containing circuit materials
  • Lead-free process compatible
  • ED and reverse treat copper foil

Applications:

  • High power RF and microwave amplifiers
  • Power amplifiers, couplers, filters, combiners, power dividers

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.060 %0.060 %D24/23; IPC-TM-650 2.6.2.1; ASTM D570
Thickness 254 - 1520 microns10.0 - 60.0 milRange of Standard Thicknesses
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 1.68 GPa244 ksiTD; 40 hours; 50%RH; ASTM D638
 2.27 GPa329 ksiMD; 40 hours; 50%RH; ASTM D638
Peel Strength 1.38 kN/m
@Temperature 288 °C,
Time 20.0 sec
7.90 pli
@Temperature 550 °F,
Time 0.00556 hour
IPC-TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmCondition A; Z direction; IPC 2.5.17.1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmCondition A; Z direction; IPC 2.5.17.1
Dielectric Constant  3.45 - 3.55
@Frequency 1e+10 Hz
3.45 - 3.55
@Frequency 1e+10 Hz
Z direction; Process; IPC-TM-650 2.5.5.5
 3.6
@Frequency 8.00e+9 - 4.00e+10 Hz
3.6
@Frequency 8.00e+9 - 4.00e+10 Hz
Z direction; Design; Differential Phase Length Method
Dissipation Factor 0.0013
@Frequency 1e+10 Hz
0.0013
@Frequency 1e+10 Hz
Z direction; IPC-TM-650, 2.5.5.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear  19.0 µm/m-°C
@Temperature -55.0 - 288 °C
10.6 µin/in-°F
@Temperature -67.0 - 550 °F
X-, Y-Direction; ASTM D3386
 39.0 µm/m-°C
@Temperature -55.0 - 288 °C
21.7 µin/in-°F
@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386
Thermal Conductivity 1.44 W/m-K
@Temperature 80.0 °C
9.99 BTU-in/hr-ft²-°F
@Temperature 176 °F
ASTM C518
Flammability, UL94 V-0V-0anticipated
 
Descriptive Properties
Dimensional Stability0.07 mm/mIPC-TM-650 2.4.3.8; X, Y direction; after etch, +E/150
 0.07 mm/mIPC-TM-650 2.4.3.9; X, Y direction; after etch, +E2/150
Thermal Coefficient of Dielectric Constant-66 ppm/°Cmod IPC-TM-650, 2.5.5.5; Z direction; -50°C to 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate
Rogers Corporation RT/duroid® 6202 High Frequency Laminate
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam

PROGA978 / 138418

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.