Entec Hylex® P2010L Polycarbonate
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Molded
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.
Information provided by Entec.
This grade is no longer in production
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
ASTM D792
Water Absorption
0.15 %
0.15 %
24 hrs; ASTM D570
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ASTM D955
Melt Flow
10
g/10 min
@Load 1.20 kg,
Temperature 300 °C
10
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
80
80
ASTM D785
Tensile Strength at Break
60.7
MPa
8800
psi
ASTM D638
Elongation at Break
110 %
110 %
ASTM D638
Flexural Strength
83.4
MPa
12100
psi
ASTM D790
Flexural Modulus
2.28
GPa
330
ksi
ASTM D790
Izod Impact, Notched
7.47
J/cm
14.0
ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
129
°C
265
°F
Unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
271
-
282
°C
520
-
540
°F
Middle Barrel Temperature
277
-
288
°C
530
-
550
°F
Front Barrel Temperature
282
-
299
°C
540
-
570
°F
Nozzle Temperature
277
-
299
°C
530
-
570
°F
Melt Temperature
288
-
316
°C
550
-
600
°F
Mold Temperature
76.7
-
93.3
°C
170
-
200
°F
Drying Temperature
121
°C
250
°F
Dry Time
3
-
12
hour
3
-
12
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Injection Pressure
6.89
-
12.4
MPa
1000
-
1800
psi
Back Pressure
0.483
-
1.03
MPa
70.0
-
150
psi
Shot Size
40 - 60 %
40 - 60 %
Screw Speed
40
-
70
rpm
40
-
70
rpm
Descriptive Properties
Holding Pressure
700 to 1200 psi
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
Entec Hylex® P2007L Polycarbonate
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
PENT068 / 36105
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.