MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Carbothane® PC-3585A-B20 Aliphatic TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Radiopaque Grade – 20% loading of Barium Sulfate

Features: Medical Grade Aliphatic Polycarbonate-based TPUs which do not yellow, with excellent oxidative stability, good mechanical properties, very good chemical resistance, radiopacity and can be color-matched

Process: Extrusion, Injection Molding or Solution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in1”x.25”x6” bar; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM D412
Elongation at Break 410 %410 %ASTM D412
100% Modulus 5.52 MPa
@Strain 100 %
800 psi
@Strain 100 %
ASTM D412
200% Modulus 10.3 MPa
@Strain 200 %
1500 psi
@Strain 200 %
ASTM D412
300% Modulus 28.3 MPa
@Strain 300 %
4100 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0152 GPa2.20 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 56.0 °C133 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 °C392 °FInjection
Front Barrel Temperature 210 °C410 °FInjection
Nozzle Temperature 220 °C428 °FInjection
Zone 1 182 °C360 °FExtrusion
Zone 2 188 °C370 °FExtrusion
Zone 3 193 °C379 °FExtrusion
Zone 4 199 °C390 °FExtrusion
Adapter Temperature 204 °C399 °FExtrusion
Die Temperature 204 °C399 °FExtrusion
Melt Temperature 210 °C410 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® AC-4095A-B20 Aromatic TPU
Lubrizol LifeSciences Carbothane® AC-4085A-B20 Aromatic TPU
Lubrizol LifeSciences Carbothane® PC-3595A-B20 Aliphatic TPU
Lubrizol LifeSciences Carbothane® PC-3585A TPU – Clear Aliphatic
Lubrizol LifeSciences Carbothane® PC-3572D TPU – Clear Aliphatic

PLUBR9007 / 203574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.