MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Carbothane® AC-4095A-B20 Aromatic TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Radiopaque Grade – 20% loading of Barium Sulfate

Features: Medical Grade Aromatic Polycarbonate-based TPU with very good mechanical properties, chemical resistance, excellent oxidative stability and can be color-matched

Process: Extrusion, Injection Molding or Solution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/in1”x.25”x6” bar; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D785
Tensile Strength, Ultimate 64.1 MPa9300 psiASTM D412
Elongation at Break 300 %300 %ASTM D412
100% Modulus 22.8 MPa
@Strain 100 %
3300 psi
@Strain 100 %
ASTM D412
200% Modulus 25.9 MPa
@Strain 200 %
3750 psi
@Strain 200 %
ASTM D412
Flexural Modulus 0.0752 GPa10.9 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 94.0 °C201 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 °C374 °FInjection
Front Barrel Temperature 200 °C392 °FInjection
Nozzle Temperature 180 °C356 °FInjection
Zone 1 199 °C390 °FExtrusion
Zone 2 204 °C399 °FExtrusion
Zone 3 210 °C410 °FExtrusion
Zone 4 210 °C410 °FExtrusion
Adapter Temperature 204 °C399 °FExtrusion
Die Temperature 204 °C399 °FExtrusion
Melt Temperature 190 °C374 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® PC-3585A-B20 Aliphatic TPU
Lubrizol LifeSciences Carbothane® PC-3595A-B20 Aliphatic TPU
Lubrizol LifeSciences Carbothane® AC-4085A-B20 Aromatic TPU
Lubrizol LifeSciences Tecoflex® EG-93A-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Pellethane® 2363-90AE TPU

PLUBR9017 / 203584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.