MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolon® 28 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: PVC Homopolymer Dispersion Resin

F-28 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities as well as low residual surfactant content. This product was designed for a diversity of application such as dip coating, slush molding, rotocasting, organosols and other areas where high strength properties are essential.

Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.30 %0.30 %ASTM D3030
Viscosity 1.2 cP1.2 cPInherent; ASTM D1243
 7000 cP7000 cPSevers, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.65 cP2.65 cPQC-10-104
Brookfield Viscosity 4500 cP4500 cP20 rpm aged 2 hrs, See note 1; SPI-VD-T1
 7000 cP7000 cP2 rpm aged 2 hrs, See note 1; SPI-VD-T1
 
Descriptive Properties
Composition0.014Methanol Extract, ASTM D2222
Gelation Temperature180°FSPI-VD-T18
K-Value75Fikentscher's Constant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolon® 10 PVC
Formosa Plastics Formolon® KVH PVC
Axiall 1601 Clear 7002 Flexible PVC
Formosa Plastics Formolon® 24A PVC
Formosa Plastics Formolon® 260 PVC

PFPCPQ098 / 150330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.