MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolon® KVH PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: PVC Homopolymer Dispersion Resin

F-KVH is a structured high molecular weight PVC homopolymer dispersion resin which imparts pseudoplastic flow in which it is used. Plastisol prepared utilizing F-KVH are particularly suited for dip, slush and rotational molding where mold release and pseudoplasticity are desired as well as fabric coating application where minimum strike through is essential.

Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.30 %0.30 %ASTM D3030
Viscosity 1.2 cP1.2 cPInherent; ASTM D1243
 8000 cP8000 cPSevers, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.65 cP2.65 cPQC-10-104
Brookfield Viscosity 60000 cP60000 cP20 rpm aged 2 hrs, See note 1; SPI-VD-T1
 500000 cP500000 cP2 rpm aged 2 hrs, See note 1; SPI-VD-T1
 
Descriptive Properties
Composition0.015Methanol Extract, ASTM D2222
Gelation Temperature175°FSPI-VD-T18
K-Value75Fikentscher's Constant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Formosa Plastics Formolon® 10 PVC
Formosa Plastics Formolon® 28 PVC
Aptek 6512-PMF Electronic grade, conductive epoxy adhesive
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade

PFPCPQ103 / 150335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.