MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMCAL TIMREX® T75 Primary Synthetic Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.

TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.

Tribological and mechanical properties:

  • High toughness
  • Good lubrication properties
Advantages and applications:
  • Low friction coefficient
  • Low wear of the counterpart and low self-wear
  • Good transfer-film formation
  • Medium electrical conductivity
  • Medium density of brushes and parts
  • Suitable for pitch-bonded and resin-bonded brushes
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.210 g/cc0.00759 lb/in³Scott
Particle Size 43 µm43 µmspringback 20.5%, pressure at 0.0477t/gg
 46 - 66 µm46 - 66 µmd90, Guaranteed
 57.5 µm57.5 µmd90, Typical
 70 µm70 µmat a density of 2.20 g/cm3
 75 µm75 µmspringback 23%, pressure at 0.0477t/gg
 145 µm145 µmspringback 24%, pressure at 0.0477t/gg
 625 µm625 µmat a density of 2.10 g/cm3
 1500 µm1500 µmat a density of 2.02 g/cm3
Specific Surface Area 9.8 m²/g9.8 m²/gBET
Deformation 1.1 %1.1 %elastic
 2.6 %2.6 %plastic
 3.7 %3.7 %plastic + elastic
Ash 0.070 %0.070 %Typical
 <= 0.10 %<= 0.10 %Guaranteed
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.35
@Temperature 850 °C,
Time 10800 sec
0.35
@Temperature 1560 °F,
Time 3.00 hour
Sintered Cu-C -brake pads with 10% TIMREX® Coke, Sinter density: 55% of the theoret. density
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.25 ohm-cm2.25 ohm-cmparticle size at 40 um, pressure at 2.5 t/cc
 2.50 ohm-cm2.50 ohm-cmparticle size at 70 um, pressure at 2.5 t/cc
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 130 W/m-K902 BTU-in/hr-ft²-°Fpowders pressed to density of 2.2 g/cm3
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.10 %0.10 %Typical
 <= 0.50 %<= 0.50 %Guaranteed
 
Descriptive Properties
Crystallite Height, Lc>100 nm
DBP absorption103 g/100 g(Dibutylphthalate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL TIMREX® KS75 Primary Synthetic Graphite
TIMCAL TIMREX® KS150 Primary Synthetic Graphite
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite
TIMCAL TIMREX® T150 Primary Synthetic Graphite

CTIMCAL27 / 2669

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.