MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMCAL TIMREX® KS75 Primary Synthetic Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.

TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.

Tribological and mechanical properties:

  • Medium toughness
  • Good lubrication properties
Advantages and applications:
  • Low friction coefficient
  • Low wear of the counterpart
  • Good transfer-film formation
  • High electrical conductivity
  • Suitable for pitch-bonded and resin-bonded brushes
  • Fe-self lubricating engineering parts
  • Fe-friction parts
  • Copper/bronze bearings
  • Copper friction parts copper clutch facings
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.240 g/cc0.00867 lb/in³Scott
Particle Size 5.0 µm5.0 µmSpringback 11.5%, pressure 0.477 t/cc
 20 µm20 µmSpringback 13%, pressure 0.477 t/cc
 23.1 µm23.1 µmd50
 55.8 µm55.8 µmd90
 48 - 65 µm48 - 65 µmd90, Guaranteed
 75 µm75 µmSpringback 17%, pressure 0.477 t/cc
 550 µm550 µmat a density of 2.16 g/cc
 1000 µm1000 µmat a density of 2.12 g/cc
Deformation 1.4 %1.4 %plastic
 1.4 %1.4 %elastic
 2.8 %2.8 %plastic + elastic
Ash 0.070 %0.070 %Typical
 <= 0.10 %<= 0.10 %Guaranteed
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.30
@Temperature 850 °C,
Time 10800 sec
0.30
@Temperature 1560 °F,
Time 3.00 hour
Sintered Cu-C -brake pads with 10% TIMREX® Coke, Sinter density: 55% of the theoret. density
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.55 ohm-cm1.55 ohm-cmparticle size 80 um, pressure 2.5 t/cc
 1.60 ohm-cm1.60 ohm-cmparticle size 42 um, pressure 2.5 t/cc
 1.80 ohm-cm1.80 ohm-cmparticle size 15 um, pressure 2.5 t/cc
 2.25 ohm-cm2.25 ohm-cmparticle size 10 um, pressure 2.5 t/cc
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.10 %0.10 %Typical
 <= 0.50 %<= 0.50 %Guaranteed
 
Descriptive Properties
Crystallite Height>100 nm
DBP absorption98 g/100g(Dibutylphthalate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hydrogenated Nitrile Rubber (HNBR)
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMCAL TIMREX® KS150 Primary Synthetic Graphite
TIMCAL TIMREX® T75 Primary Synthetic Graphite

CTIMCAL15 / 2657

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.