GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. Applications: GB311U has been developed especially for demanding applications in the automotive industry including technical components exposed to high heat and loads, washing machine parts, and structural parts.Information provided by Borealis AG |