MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Geon® Performance Solutions HC XV1144 PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Transparent

Material Notes: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is "For foods of high water content only". This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80
@Time 10.0 sec
80
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 18.5 MPa2680 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 450 %450 %Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.00827 GPa1.20 ksiType IV, 5.1 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact, Unspecified Rating
 YesYesUnspecified Rating
USP Class VI YesYes
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
FormsPellets
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesHose
 Medical Appliances
 Tubing

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible XV 1144 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable 0860-xx02D Polyvinyl Chloride, Flexible
Geon® Performance Solutions 0750-xx17D Vinyl Compound - Wire & Cable
Fainplast Compounds PH 76/A Flexible PVC, Transparent Extrusion
Fainplast Compounds PH 68/A Flexible PVC, Transparent Extrusion

PH1PN8191 / 102027

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.