MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 0750-xx17D Vinyl Compound - Wire & Cable  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes:

Description/Features:

  • UL 60°C
  • Transparent

Applications:

  • Automotive Insulation
  • Automotive Jacket
  • Telecommunication Insulation
  • Telecommunication Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 727215 sec; ASTM D2240
Tensile Strength, Yield 16.8 MPa2440 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 400 %400 %Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus 0.00793 GPa1.15 ksiType 4 - Flexibles, 20 in/min; ASTM D638
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 166 - 171 °C330 - 340 °FExtrusion
 
Descriptive Properties
Product FormPellets/Cubes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible XV 1144 Polyvinyl Chloride, Flexible
Geon® Performance Solutions HC XV1144 PVC, Flexible
Colorite Polymers Flexchem 4051-02 Vinyl Compound
Geon® Performance Solutions Vinyl Wire & Cable 0860-xx02D Polyvinyl Chloride, Flexible
Bayshore Vinyl Compounds BVC 6200-65 Vinyl Compound

PH1PO1112 / 43888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.