MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: CoPA, injection molding grade, 15% glass fibers

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 8.5 %8.5 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 2.6 %2.6 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 138 cm³/g1.38 dl/gISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiConditioned; ISO 527-1/-2
 125 MPa18100 psiISO 527-1/-2
Elongation at Break 3.0 %3.0 %ISO 527-1/-2
 12 %12 %Conditioned; ISO 527-1/-2
Tensile Modulus 3.60 GPa522 ksiConditioned; ISO 527-1/-2
 6.30 GPa914 ksiISO 527-1/-2
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Impact 64446444Puncture maximum force (N); ISO 6603-2
 585
@Temperature -30.0 °C
585
@Temperature -22.0 °F
Puncture maximum force (N); ISO 6603-2
Puncture Energy 4.00 J2.95 ft-lbISO 6603-2
 3.00 J
@Temperature -30.0 °C
2.21 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 3.00 J
@Temperature -30.0 °C
2.21 ft-lb
@Temperature -22.0 °F
Conditioned; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmConditioned; IEC 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
Conditioned; IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
 40.0 kV/mm1020 kV/inIEC 60243-1
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 0.12
@Frequency 1e+6 Hz
0.12
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 0.20
@Frequency 100 Hz
0.20
@Frequency 100 Hz
Conditioned; IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
Melting Point 213 °C415 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 60.0 °C140 °FISO 75-1/-2
Vicat Softening Point 200 °C392 °F50°C/h 50N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
Oxygen Index 22 %22 %ISO 4589-1/-2
 
Descriptive Properties
AdditivesRelease agent
FormPellets
ISO Short NameISO 1874-PA 6/66, MR, 14-060, GF15
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omnia Plastica Omniamid PA6 G - G - at 50% RH
Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 15 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 115 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned

PLANX0749 / 98964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.