MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, 30% glass fibers, injection molding

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %50% RH; ISO 62
Water Absorption at Saturation 7.0 %7.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0016 cm/cm0.0016 in/in150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0082 cm/cm0.0082 in/in150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 260 °C
14 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa14500 psiISO 2093-1
Tensile Strength at Break 105 MPa15200 psi5 mm/min; ISO 527-1,-2
Elongation at Break 6.0 %6.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 6.10 GPa885 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 170 MPa24700 psi2 mm/min; ISO 178-A
Flexural Yield Strength 145 MPa
@Strain 3.5 %
21000 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 5.10 GPa740 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 6.0 %6.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  70.0 kJ/m²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy  5.00 J
@Temperature -30.0 °C
3.69 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 14.0 J
@Temperature 23.0 °C
10.3 ft-lb
@Temperature 73.4 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 5100 MPa740000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 4100 MPa595000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant  5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.12
@Frequency 1e+6 Hz
0.12
@Frequency 1e+6 Hz
IEC 60250
 0.20
@Frequency 100 Hz
0.20
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °Finjection molding
 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 120 °C176 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry

PLANW9375 / 208196

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.