MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric strength, moisture resistance, and physical toughness make Mylar® EL21 a very versatile and functional insulating material.

General Product Info: Mylar® EL21 films offer high dielectric strength, good chemical resistance, and exceptional durability in high-temperature environments

Typical Applications: Mylar® type EL21 films, similar to Mylar® type MO films, are heavy gauge insulating films designed for general purpose electrical/electronic applications, such as transformers, laminates, bus bars, and punched parts.

Approvals: UL 94 VTM-2 - for 92-1400 gauge(0.023-0.35 mm) and UL Recognition - for 92-500 gauge (0.023-0.13mm) HWI=5, HAI=4, CTI=1;for 700-1400 gauge (0.18-0.35mm) HWI=4, HAI=0, CTI=1

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.3925 g/cc0.050307 lb/in³
Thickness 254 microns10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882A
Film Elongation at Break, TD 140 %140 %ASTM D882A
Film Tensile Strength at Break, MD 186 MPa27000 psiASTM D882A
Film Tensile Strength at Break, TD 200 MPa29000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 74.8 kV/mm1900 kV/in1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 19000 V19000 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
Comparative Tracking Index 400 - 600 V400 - 600 V
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 sec
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcs
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Shrinkage, MD 1.5 %
@Temperature 150 °C,
Time 1800 sec
1.5 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.1 %
@Temperature 150 °C,
Time 1800 sec
1.1 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Optical Density 4242[%]
 
Descriptive Properties
Yield (nominal)2000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge
DuPont Teijin Films Mylar® LBTW Polyester Film, 75 Gauge

PDTZ9328 / 139648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.