MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® LBTW Polyester Film, 75 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commercially available in nominal 48, 75 and 92 gauges. Mylar® LBTW is wound inverted with the corona-treated side facing the outside of the roll

General Product Info: In addition to the enhanced wettability offered to inks, primers, adhesives and coatings, Mylar® LBTW offers all of the properties attributed to Mylar® LB, including high levels of strength, temperature resistance and flavor and odor barriers. Its sparkling clarity and insensitivity to humidity make Mylar® LBTW a preferred print carrier.

Typical Applications: Mylar® LBTW typically is used as the reverse printed outer ply of a lamination with inner plies providing additional oxygen barrier if needed, as well as heat sealability. The availability of the two-side corona-treated Mylar® LBT2 permits use where the ply will be buried inside a lamination with bonding to both surfaces or where the exposed outer surface will subsequently receive surface printing, code dating or some for of package lot identification.

Approvals: FDA Food Contact Status - All gauges of Mylar® LBTW comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, sections (f), (g) and (h). These regulations describe films that can safely be used in contact with all types of foods including alcoholic beverages that do not exceed 50% alcohol by volume. The films listed above can be used to contain foods during oven cooking at temperatures up to and above 250°F. The films listed above may be used for packaging, transporting, or holding alcoholic beverages that do not exceed 50% alcohol by volume. UL Recognition - Product has been registered with Underwriters Laboratories. UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm) UL Recognition - for 92 - 500 gauge (0.023 - 0.13mm) - HWI=5, HAI=4, CTI=1

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Water Vapor Transmission 29.5 g/m²/day
@Temperature 38.0 °C
1.90 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 19.0 microns0.750 mil
Coating Weight 25.9 g/m²16.2 lb/ream0.5 m2; ASTM E252
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 130 %130 %ASTM D882A
Film Elongation at Break, TD 100 %100 %ASTM D882A
Tensile Modulus 3.79 GPa550 ksiASTM D882
Graves Tear Strength 0.158 kN/m0.900 pliASTM D1004
Film Tensile Strength at Break, MD 200 MPa29000 psiASTM D882A
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 - 600 V400 - 600 V
Hot Wire Ignition, HWI <= 7.0 sec<= 7.0 sec
High Amp Arc Ignition, HAI <= 15 arcs<= 15 arcs
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Shrinkage, MD 2.2 %
@Temperature 150 °C,
Time 1800 sec
2.2 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.1 %
@Temperature 150 °C,
Time 1800 sec
1.1 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Haze 6.5 %6.5 %ASTM D1003
Gloss 180 %180 %20°; ASTM D2457
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)7 cc/100 in2O2, 24 hr; ASTM D3985 (77°F/75% RH/1 ATM)
Yield (nominal)26700 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge

PDTZ9338 / 139658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.