MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 1943 Impact Modified Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and chemical properties provided with the polyamide backbone.

Capron 1943 is generally recommended for applications such as cellular phone housings, handheld device, caps, furniture rails, escutcheons, covers, mower decks and tool.

Data provided by Allied Signal.

Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-280 degC (464-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO data
Melt Density 0.938 g/cc
@Temperature >=220 °C
0.0339 lb/in³
@Temperature >=428 °F
Moisture Absorption at Equilibrium 2.4 %2.4 %50% RH; 23°C; ISO data
Water Absorption at Saturation 8.6 %8.6 %in water; 23°C; ISO data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 69.0 MPa10000 psiISO value at 50 mm/min.
 70.0 MPa10200 psiASTM value at 50 mm/min.
Elongation at Break >= 50 %>= 50 %Nominal
 70 %70 %Nominal
Flexural Yield Strength 95.0 MPa13800 psiASTM Data
Flexural Modulus 2.39 GPa347 ksiASTM Data
Poissons Ratio 0.350.35ISO data
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 3.89 J/g-°C0.930 BTU/lb-°FMelt value
Thermal Conductivity 0.168 W/m-K1.17 BTU-in/hr-ft²-°FMelt
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM Data
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
Overview of materials for Nylon 6, Cast
Overview of materials for Nylon 6, Impact Grade
BASF Ultramid® 8255 HS PA6 (Conditioned)
BASF Ultramid® 8253 PA6 (Dry)

PALC03 / 23791

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.