MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Daikin POLYFLON™ PTFE M-12 Polytetrafluoroethylene Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Daikin-Polyflon™ M-12 is a polytetrafluoroethylene virgin granular fine cut resin. This general purpose molding powder has been specifically designed for use in small to medium billet compression molding. It is particularly well suited to thin skived film applications requiring excellent physical and electrical properties.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 - 2.18 g/cc2.15 - 2.18 g/ccASTM D 4894
Bulk Density >= 0.300 g/cc>= 0.0108 lb/in³ASTM D 4894
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 35.0 MPa>= 5080 psiASTM D 4894
Elongation at Break >= 350 %>= 350 %ASTM D 4894
Compressive Yield Strength 7.60 MPa1100 psi0.2% offset; ASTM D695
 5.00 MPa
@Strain 1 %
725 psi
@Strain 1 %
ASTM D695
 28.2 MPa
@Strain 25 %
4090 psi
@Strain 25 %
ASTM D695
Compression Set  8.8 %
@Pressure 13.7 MPa,
Time 90000 sec
8.8 %
@Pressure 1990 psi,
Time 25.0 hour
ASTM D621
 15.3 %
@Pressure 6.90 MPa,
Time 720000 sec
15.3 %
@Pressure 1000 psi,
Time 200 hour
ASTM D621
 18.5 %
@Pressure 13.7 MPa,
Time 360000 sec
18.5 %
@Pressure 1990 psi,
Time 100 hour
ASTM D621
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant <= 2.1
@Frequency 1000 Hz
<= 2.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength >= 90.0 kV/mm
@Thickness 0.100 mm
>= 2290 kV/in
@Thickness 0.00394 in
Dielectric Loss Index <= 0.00010
@Frequency 1000 Hz
<= 0.00010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °F
Maximum Service Temperature, Air 260 °C500 °F
Shrinkage 2.7 - 3.7 %2.7 - 3.7 %ASTM D4894
 
Descriptive Properties
AppearanceWhite Powder
MIT Flex7,000,000 cyclesASTM D2178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 7A Granular Molding Powder
Daikin POLYFLON™ PTFE M-111 Polytetrafluoroethylene Molding Powder
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Daikin POLYFLON F-201 PTFE Fine Powder
Dalau Dalcon 001 100% Virgin PTFE

PDAIJ9874 / 209945

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.