MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Tape™ 682-TB1-2 Thermal Barrier Ceramic Tape
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: The 682-TB tape is a woven silica fabric tape used with temperature resistance as high as 2500 °F used to offer thermal insulation for pipes. The Pyro-Tape™ 682-TB has an adhesive backing which is used to ease wrapping around pipes. The adhesive will burn off at 275 °F, and then the tape is secured to the pipe in intervals with stainless steel wire.
Available in 1, 2, and 4 inch widths.

Vendors: Aremco’s Pyro-Tape 682-Series high temperature tapes are ideal for abrasion, chemical, electrical, and thermal insulation. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Thickness 760 microns29.9 mil
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.144 W/m-K
@Temperature 316 °C
1.00 BTU-in/hr-ft²-°F
@Temperature 600 °F
 
Descriptive Properties
Silica>96%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 912-10R12-P1 0.012" (0.305 mm) Self-Fusing Silicone Tape
Rogers Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape
Aremco Pyro-Tape™ 682-TB2-1 Thermal Barrier Ceramic Tape
3M Nextel™ BP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ BP-18 Woven Tape 312 (3.8 cm)

CAREM995 / 138452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.