MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape
Categories: Polymer; Thermoset; Silicone

Material Notes: Design/Construction:
Interleave: Polyethylene
Rubber: Cured Self-fusing Silicone Rubber
Cross Section Type: 1” Wide Rectangular

1 inch wide, 10 mil thick, Gray, Rectangular cross-section, Self-fusing silicone tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length in yards.

Meets US Military Specification A-A-59163(supercedes Mil-I-46852C) except for packaging and sampling. The following tests are conducted on one roll from each lot of tape: Thickness, Width, Bond Strength, Tensile Strength, Elongation, Dielectric Strength, and Water Absorption.

Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.

Performance Advantages:
Resists moisture, oxygen, and ozone to assure continuous high insulation values.
Conforms smoothly when wrapped around complex forms.
Bonds to itself at room temperature within 24 hours.
Remains non-tacky to the touch and does not adhere to other surfaces, or substrates.
Insulates with single wrap, thereby reducing labor time and cost.
Dampens vibration and resists heat and mechanical shock as well as corona.
Inherently flame resistant and when burned forms a non-conductive ash.
SA & SB MOX-Tapes® provide a uniform thickness even around sharp edges. Fiberglass fabric, encapsulated inside the silicone rubber, prevents wicking and maintains high insulation resistance under high humidity conditions. These controlled stretch tapes provide a uniform insulation barrier.
All tapes are protected by a special interleaved liner.

Applications:

    Mechanical:
  • Protection of coils from vibration.
  • Vibration fixture, anti-scratch, and clamping pads.
  • Harness wrapping and wire bundling, including for high temperature applications.
  • Applied to rollers for protection and traction.
  • Plant maintenance.
  • Superior, heavy duty repair tape for emergency insulating barrier.
    Electrical:
  • Insulation of field armature and interpole coils in large motors.
  • Insulation for splicing and terminating of wire and cable.
  • Insulating and sealing electrical connections.
  • Insulating coil leads and bus bar connections.
  • Electromagnetic coil insulation.
  • Motor connections.
  • Overwrapping of deteriorated insulation in reclaimed motors.
    Environmental:
  • On-board aviation and space applications.
  • Underground cable splices.
  • Insulating heated transfer lines.
  • Insulating in radioactive environments.
  • Masking agent utilized in manufacturing processes and powder coatings.
  • Insulating, protecting, and sealing rigging hardware and power systems in marine applications.

This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.1 %1.1 %Arlon SQA-TMS-016
Thickness 76.2 microns3.00 milPolyethylene, Interleave
 254 microns10.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Silicone Property; ASTM D2240
Tensile Strength 7.481 MPa1085 psiSilicone Property; ASTM D412
Elongation at Break 495 %495 %Silicone Property; ASTM D412
Peel Strength 0.403 kN/m2.30 pliBond Strength; Arlon SQA -TMS-015
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm763 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
From date of manufacture
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 912-10R12-P1 0.012" (0.305 mm) Self-Fusing Silicone Tape
Aremco Pyro-Tape™ 682-TB2-1 Thermal Barrier Ceramic Tape
Aremco Pyro-Tape™ 682-TB1-2 Thermal Barrier Ceramic Tape
3M Nextel™ BP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ BP-18 Woven Tape 312 (3.8 cm)

PARL440 / 125626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.