MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
Water Absorption 1.2 %1.2 %ASTM D570
Linear Mold Shrinkage 0.018 cm/cm0.018 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 44.8 MPa6500 psiASTM D638
Tensile Strength, Yield 46.9 MPa6800 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Yield Strength 65.5 MPa9500 psiASTM D790
Flexural Modulus 1.79 GPa260 ksiASTM D790
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 216 °C421 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 °C490 °F
Middle Barrel Temperature 268 °C515 °F
Front Barrel Temperature 285 °C545 °F
Nozzle Temperature 266 - 282 °C510 - 540 °F
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 26.7 - 93.3 °C80.0 - 200 °F
Drying Temperature 71.1 °C160 °F
Dry Time 4 hour4 hour
Injection Pressure 68.9 MPa10000 psi
Back Pressure 0.0689 - 0.689 MPa10.0 - 100 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 153HSL NC010 PA612
Overview of materials for Nylon 66, Impact Grade
Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6
Adell AD-30 Nylon 66, Ultra High Impact

PZ9PT54 / 21503

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.