MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact; PVC, Rigid Grade

Material Notes: Features: High Impact Resistance; Medium Gloss

Processing Method: Extrusion

Forms: Pellets

Additional Information: Performance Characteristics: Yellow Card, Interior, Medium Gloss, Excellent Finish

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 808010 seconds; ASTM D2240
Tensile Strength at Break 44.9 MPa6510 psiASTM D638
Tensile Strength, Yield 45.0 MPa6520 psiASTM D638
Elongation at Break 54 %54 %ASTM D638
Elongation at Yield 3.1 %3.1 %ASTM D638
Tensile Modulus 2.38 GPa345 ksiASTM D638
Flexural Modulus 2.68 GPa389 ksiASTM D790
Izod Impact, Notched 7.47 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
14.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 103 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
0.192 ft-lb/mil
@Thickness 0.125 in,
Temperature 73.0 °F
Procedure B, 0.250" Conical Dart; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C
@Thickness 3.17 mm
157 °F
@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 5VA5VA
 V-0
@Thickness 22.9 mm
V-0
@Thickness 0.900 in
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Arkema Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
Karina 802-18/462-C-ERB Gray PVC Compound
Teknor Apex Sinvicomp SRF 3703 Polyvinyl Chloride, Rigid
AlphaGary Dural 725C CLEAR 0003 Full Rigid Polyvinyl Chloride Compound

PTEKNO689 / 128867

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.