MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polycarbonate POL051G20L Glass Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inMD; ASTM D955
Melt Flow 10 g/10 min10 g/10 minASTM D1238
Ash 20 %20 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 100 MPa14500 psiASTM D638
Tensile Strength, Yield 102.0 MPa14790 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 4.100 GPa594.6 ksiASTM D638
Flexural Strength 170.0 MPa24650 psiASTM D790
Flexural Modulus 5.999 GPa870.1 ksiASTM D790
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 144 °C291 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced
Covestro Makrolon® 2405 MAS056 Polycarbonate
Overview of materials for Polycarbonate, Optical Grade
Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact
Bamberger Polymers Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade

PACLO100 / 22355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.