MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers TEKAMID® TA210L Lubricated PA66, DAM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Lubricated

Information provided by E-Polymers Co. Ltd.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.3 %1.3 %23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7878ASTM D786
Hardness, Rockwell R 120120ASTM D786
Hardness, Shore D 7979
Tensile Strength, Yield 85.0 MPa12300 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Yield Strength 117 MPa17000 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiASTM D790
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 190 sec190 secTungsten electrode; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 260 °C500 °FASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 230 °C446 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FASTM D648
Flammability, UL94 V-2V-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 280 °C518 - 536 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
Aluminum, Al

PEPOLY00 / 36302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.