MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
E-Polymers TEKAMID® TA210L Lubricated PA66, DAM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Lubricated

Information provided by E-Polymers Co. Ltd.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.3 %23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 78ASTM D786
Hardness, Rockwell R 120ASTM D786
Hardness, Shore D 79
Tensile Strength, Yield 85.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Yield Strength 117 MPaASTM D790
Flexural Modulus 3.00 GPaASTM D790
Izod Impact, Notched 0.550 J/cmASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 190 secTungsten electrode; ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.250 W/m-K
Melting Point 260 °CASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 230 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CASTM D648
Flammability, UL94 V-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °C
Mold Temperature 40.0 - 60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
Aluminum, Al

PEPOLY00 / 36302

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.