MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel the top layer of the product. Full cure will occur over time at room temperature even in shadow areas. Due to the acrylate reaction, the catalyzed resin warms slightly to about 32oC nearly instantaneously.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccPart B; TM R050-16
 1.10 g/cc1.10 g/ccMixed; TM R050-16
 1.14 g/cc1.14 g/ccPart A; TM R050-16
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
TM R050-35
Viscosity 1500 cP1500 cPPart B, RVT, #2, 20 rpm; TM R050-12
 3000 cP3000 cPMixed; TM R050-12
 3500 cP3500 cPPart A, RVT, #3, 20 rpm; TM R050-12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080TM R050-17
Tensile Strength at Break 31.0 MPa4500 psiTM R050-36
Tensile Strength, Ultimate 31.7 MPa4600 psiTM R050-36
Tensile Strength, Yield 20.7 MPa3000 psiTM R050-36
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %TM R050-36
Tensile Modulus 2.07 GPa300 ksiTM R050-36
Compressive Yield Strength 41.4 MPa6000 psiTM R050-38
Compressive Strength 103 MPa15000 psiBreak; TM R050-38
 138 MPa20000 psiUltimate; TM R050-38
Compressive Modulus 2.07 GPa300 ksiTM R050-38
Adhesive Bond Strength 20.7 MPa3000 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cm
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
4.5
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm440 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°F
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 54.0 °C129 °FTM R050-25
 
Processing PropertiesMetricEnglishComments
Pot Life 15 - 30 min15 - 30 minMass: 50g; TM R050-19
 
Descriptive Properties
ColorClear
Mix Ratio2:1Volume
 215:100Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resin Technology Group UV-422 Flexible, UV Curing Sealant
Permabond UV7141 UV-curable Adhesive
Henkel Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive

PRESL137 / 101551

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.