MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group UV-422 Flexible, UV Curing Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substrates and a wide variety of other substrates such as metals, epoxy-board, glass and other plastics in sealing and tacking applications. UV 422 forms shock absorbing bonds. Uses include flexible coatings and encapsulation.

Applications:

Transducer mountings, Switch potting, Connector sealing, Automotive components, Wire tacking.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccUncured
 1.15 g/cc1.15 g/ccOf cured material
Water Absorption 0.43 %0.43 %Cured
Viscosity 3000 - 4000 cP
@Temperature 25.0 °C
3000 - 4000 cP
@Temperature 77.0 °F
Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 7065 - 70Cured
Tensile Strength at Break 11.7 MPa1700 psiCured
Elongation at Break 250 %250 %Cured
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
Cured
Maximum Service Temperature, Air 177 °C351 °FCured
Minimum Service Temperature, Air -54.0 °C-65.2 °FCured
Flash Point >= 93.3 °C>= 200 °FUncured
Shrinkage 6.8 %6.8 %Upon cure, by volume
 
Descriptive Properties
ColorClear/Light Straw Liquid
CompositionUrethane Oligomer/ (Meth) Acrylate Monomer Blend
SolubilityAlcohol, Chlorinated solvents
ToxicityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Permabond UV7141 UV-curable Adhesive
Henkel Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive

PRESINT645 / 65529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.