MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ZEON Nipol® 1072 Carboxylated Nitrile Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nipol 1072 is a copolymer of butadiene and acrylonitrile with medium oil resistance, modified to contain free carboxylic groups. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.

Oil resistant mechanical goods with outstanding abrasion resistance. Carboxyl content is 0.075 EPHR.

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/cc
Viscosity 200 - 5000 cP200 - 5000 cPUnmilled Cement; Zeon Test #1377
Mooney Viscosity 40 - 55
@Temperature 100 °C
40 - 55
@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.80 %<= 0.80 %Zeon Test #873
 
Descriptive Properties
AO TypeNS
Bound ACN (%, acrylonitrile)26-28
Carboxyl Content, %0.07-0.08
Heat Loss (%) Max0.5
Hot/ColdC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ZEON Nipol® 1072CGX Carboxylated Nitrile Elastomer
ZEON Nipol® 1022 Nitrile Elastomer
ZEON Nipol® 1072x28 Carboxylated Nitrile Elastomer
Dow Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
ZEON Nipol® NX775 Carboxylated Nitrile Elastomer

PZEONB61 / 73020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.