MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Categories: Metal; Nonferrous Metal; Bismuth Alloy; Solder/Braze Alloy

Material Notes: Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.

Information Provided by Indium Corporation

Key Words: lead free, eutectic solder
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.56 g/cc0.309 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 23
@Load 4.00 kg
23
@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 55.2 MPa8010 psi
Elongation at Break 55 %55 %% elongation on 5.65 (sq. root Area) gauge length
Shear Strength 3.40 MPa493 psiShear Bond Holding Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000380 ohm-cm0.0000380 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 44.8 J/g19.3 BTU/lb
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 °C
8.33 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C0.0399 BTU/lb-°FSolid
 0.201 J/g-°C0.0480 BTU/lb-°FLiquid
Thermal Conductivity 19.0 W/m-K
@Temperature 85.0 °C
132 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 138 °C280 °FEutectic
Solidus 138 °C280 °F
Liquidus 138 °C280 °F
 
Component Elements PropertiesMetricEnglishComments
Bismuth, Bi 58 %58 %
Tin, Sn 42 %42 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy
Overview of materials for Low Alloy Steel
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy
Overview of materials for Medium Alloy Steel
Overview of materials for Stainless Steel

NNIN14 / 18470

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.