MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dynasol Solprene® 1106 Solution Styrene-Butadiene Rubber (SSBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Solprene® 1106 is a linear high molecular weight random-block styrene/butadiene copolymer with 10% styrene, 6% present as a polystyrene block. This grade has a non-staining antioxidant system; FDA approved for use in food contact applications and is essentially gel free with a very clear color. It is packed in bales with a low melting point polyethylene wrapping.

Uses: Solprene 1106 is mainly used as an impact modifier in polystyrene products.

Applications: Plastic modification

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccDIN 53479
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Viscosity 42 cP42 cP5% Styrene solution; NM-300-32
 
Chemical PropertiesMetricEnglishComments
Styrene Content >= 6.0 %>= 6.0 %Block; NM 202-07
 10 %10 %ASTM D5775
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Color<10Apha, NM 300-33
Insolubles<0.1%NM 300-15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Synthos SPRINTAN™ SLR 4630 Solution Styrene Butadiene Rubber (S-SBR)
Dow SE SLR-4630 Solution polymerized Styrene Butadiene Rubber (S-SBR)

PDYNA981 / 132976

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.