MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow SE SLR-4630 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SE SLR-4630 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of TDAE oil in relation to solid rubber. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and non-staining stabilized. SE SLR-4630 is used in the tire industry for the manufacture of winter and all season applications. It can also be used for the manufacture of high-quality technical rubber articles. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film. At mixing temperatures above 110°C, the rubber can be processed with the packaging film.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement  2.8
@Temperature 160 °C
2.8
@Temperature 320 °F
[dNm]; ML, (0.5 RAD); ASTM D5289
 4.4
@Temperature 160 °C
4.4
@Temperature 320 °F
[min]; ts1, (0.5 RAD); ASTM D5289
 10.9
@Temperature 160 °C
10.9
@Temperature 320 °F
[min]; T50, (0.5 RAD); ASTM D5289
 14.3
@Temperature 160 °C
14.3
@Temperature 320 °F
[dNm]; MH, (0.5 RAD); ASTM D5289
 17.9
@Temperature 160 °C
17.9
@Temperature 320 °F
[min]; T90, (0.5 RAD); ASTM D5289
Mooney Viscosity 55
@Temperature 100 °C
55
@Temperature 212 °F
[MU]; ML 1+4, unmassed sample; ASTM D1646
Vinyl Acetate Content 63 %63 %FTIR, internal method
Collected Volatile Condensable Material 0.32 %0.32 %ASTM D5668
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Chemical PropertiesMetricEnglishComments
Styrene Content 25 %25 %FTIR, internal method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 56.7
@Thickness 12.5 mm
56.7
@Thickness 0.492 in
(25 min / 160°C); ASTM D2240
Tensile Strength, Ultimate 20.0 MPa2900 psiDie C (35 min / 145°C); ASTM D412
Tensile Stress at Strain 10.5 MPa
@Strain 300 %
1520 psi
@Strain 300 %
ASTM D412
Elongation at Break 540 %540 %ASTM D412
Rebound 19 %
@Thickness 12.5 mm
19 %
@Thickness 0.492 in
Schob pendulum, (25 min / 160°C); ISO 4662
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 92.2 °C198 °F
Glass Transition Temp, Tg -28.9 °C-20.0 °FHR 10 K/min; half height; DSC
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month>= 12.0 Month
 
Descriptive Properties
Accelerator (TBBS) wt%1.38ASTM 3185-2B
Carbon Black wt%68.75ASTM 3185-2B; IRB 7
Stearic Acid wt%1ASTM 3185-2B
Sulfur content, %1.75ASTM 3185-2B
Total Extractables %27.4ASTM D5774
Zinc Oxide wt%3ASTM 3185-2B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Buna® SB 1500 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Dow Buna® SB 1723 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Dow Buna® SB 1739 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Chemours Viton® F-605C Fluoroelastomer (FKM)
Chemours Viton® A-201C Fluoroelastomer (FKM)

PDOW1105 / 30309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.