MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient FireCon™ CPE 30-11 RoHS BLACK Polyethylene, Chlorinated (CPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: CPE-30-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 RoHS BLACK offers high tensile and superior fluid resistance.

Note: Pre-drying is recommended for 4 hours at 175°-185°F. Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment. NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 414110 sec; ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 350 %350 %Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.00827 GPa1.20 ksiType IV, 510 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
Oxygen Index 30 %
@Thickness 1.91 mm
30 %
@Thickness 0.0752 in
ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
FeaturesFlame Retardant
FormsPellets
Generic MaterialCPE
Generic NamePolyethylene, Chlorinated (CPE)
Regional AvailabilityAsia Pacific
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesCable Jacketing
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 1240 UV RoHS NATURAL Polyethylene, Chlorinated (CPE)
Avient Syncure™ V0045G RoHS Polyethylene, Crosslinked (XLPE)
Avient FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE)

PH0POL1043 / 145612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.