MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-5-5-8-3 (Ti-5Mo-5V-8Cr-3Al), 0.25 mm Foil
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Relative to ASTM Gr. 20, Ti-3-8-6-4-4. Characterized by cold formable and weldable high strength Ti alloy.

Applications:

  • Bars for deep well strings in the petroleum industry
  • Sheets thickness between 3.0-4.0 mm for knives used in the sea (hardness min. HRC40 in aged state)
  • Sheets for high strength application in aerospace and airspace industry
  • Ultra high velocity centrifugal rotor

Data provided by MarkeTech International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.80 g/cc0.173 lb/in³estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1000 MPa145000 psiAnnealed
 1230 MPa178000 psiAged Condition 3
 1280 MPa186000 psiAged Condition 2
 1400 MPa203000 psiAged Condition 1
Elongation at Break 4.0 %4.0 %Aged Condition 1
 9.0 %9.0 %Aged Condition 2
 15 %15 %Annealed
 18 %18 %Aged Condition 3
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Chromium, Cr 8.0 %8.0 %
Molybdenum, Mo 5.0 %5.0 %
Titanium, Ti 79 %79 %
Vanadium, V 5.0 %5.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-5-5-8-3 (Ti-5Mo-5V-8Cr-3Al), 1 to 3 mm Sheet
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265)
Titanium Beta CEZ Unaged
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel
ATI Allegheny Ludlum K12® Dual Hardness Steel

MTBODB / 14217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.