MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BLUESTAR PBT 1100
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses good chemical resistance, abrasive resistance, low friction factor and extremely low hygroscopicity, as well as good electrical, thermal and mechanical properties and processability. Primary applications include brushes (in blends with PET); color masterbatches, extrusion into sheets or films; optical cable, and after reinforcement and modification, the products can be widely used in more fields as electronics and electricity, automobiles, communication, IT, lighting, household appliances, commercial machines, machinery and other industries.

CAS No: 30965-26-5 or 26062-94-2

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 - 1.33 g/cc1.29 - 1.33 g/ccDipping/distilled water; ISO 1183
Moisture Absorption at Equilibrium <= 0.3 %<= 0.3 %Loss on drying; ISO 15512
Viscosity Measurement 0.98 - 1.020.98 - 1.02Intrinsic Viscosity, Phenol-tetrachloroethane; ISO 1628-5
Melt Flow 30 - 45 g/10 min
@Load 2.16 kg,
Temperature 250 °C
30 - 45 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Ash <= 0.035 %<= 0.035 %Calcination; ISO 3451-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 - 226 °C432 - 439 °F10°C/min; ISO11357 (DSC)
 
Descriptive Properties
Carboxyl End Groups<30 mol/tPhenol-chloroform dissolvent, Potentiometric titration
Color B<6.0Pellet, C/2° light, Hunter Lab photometer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PBT-1100 PBT Resin
Beijing Ranger Chem BLUESTAR® 1110 PBT
Gromax PBT 1100-211L
BASF Ultradur® B 6550 PBT
BLUESTAR PBT 1100A

PBLUE903 / 135326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.