MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Ranger Chem BLUESTAR® 1110 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Can be used directly for spinning, or it can be used after reinforcement & compounding. It can also be used to produce cable sheath through tackification

Information provided by Beijing Ranger Chemical Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.31 g/cc0.0470 - 0.0473 lb/in³ISO 1183
Viscosity Test 1.08 - 1.12 cm³/g0.0108 - 0.0112 dl/gQ/NHS501
Melt Flow 18 - 28 g/10 min18 - 28 g/10 minISO 1133
 
Chemical PropertiesMetricEnglishComments
Carboxyl End Groups 0.030 meq/kg0.030 meq/kgQ/NHS501
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 - 60.0 MPa7250 - 8700 psiISO 527
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 225 °C428 - 437 °F
Moisture Content 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Ranger Chem BLUESTAR® 1084 PBT
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer
Beijing Ranger Chem BLUESTAR® 1135 PBT
Beijing Ranger Chem BLUESTAR® 1079 PBT
Beijing Ranger Chem BLUESTAR® 1120 PBT

PRANG129 / 93134

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.