MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Femur
Categories: Wood and Natural Products

Key Words: Bone, leg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 12.0 GPa1740 ksiradial direction
 13.4 GPa1940 ksitangential direction
 20.0 GPa2900 ksilongitudinal direction
Compressive Modulus 11.7 GPa1700 ksitangential direction
 11.7 GPa1700 ksiradial direction
 18.2 GPa2640 ksilongitudinal direction
Poissons Ratio 0.220.22in tension radial-longitudinal
 0.240.24in tension, tangential-longitudinal
 0.380.38in tension, radial-tangential
 0.630.63in compression, radial-tangential
Shear Modulus 4.50 GPa653 ksiin tension, radial-tangential
 5.60 GPa812 ksiin tension, radial-longitudinal
 6.20 GPa899 ksiin tension, tangential-longitudinal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Human Compact Bone, Haversian System
Cortical Bone
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Titanium, Ti
Sawbones Third-Generation Simulated Cortical Bone

PTSXBI20 / 71506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.