MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Femur
Categories: Wood and Natural Products

Key Words: Bone, leg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 12.0 GParadial direction
 13.4 GPatangential direction
 20.0 GPalongitudinal direction
Compressive Modulus 11.7 GPatangential direction
 11.7 GParadial direction
 18.2 GPalongitudinal direction
Poissons Ratio 0.22in tension radial-longitudinal
 0.24in tension, tangential-longitudinal
 0.38in tension, radial-tangential
 0.63in compression, radial-tangential
Shear Modulus 4.50 GPain tension, radial-tangential
 5.60 GPain tension, radial-longitudinal
 6.20 GPain tension, tangential-longitudinal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Human Compact Bone, Haversian System
Cortical Bone
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Titanium, Ti
Sawbones Third-Generation Simulated Cortical Bone

PTSXBI20 / 71506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.