MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper nickel 30%, UNS C71500, OSO25 Temper 25 mm tubing
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Good hot and cold workability. Fabricated by forming and bending, welding.

Applications: condensers, condenser plates, distiller tubing, evaporator and heat exchanger tubing, ferrules, salt water piping.

Test specimen: tubing - 25mm OD x 1.65mm wall thickness.

Key Words: CDA 715 (70/30); 70-30 Cupronickel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4545
Tensile Strength, Ultimate 415 MPa60200 psi
Tensile Strength, Yield 170 MPa
@Strain 0.5 %
24700 psi
@Strain 0.5 %
Elongation at Break 45 %45 %In 50 mm
Modulus of Elasticity 150 GPa21800 ksi
Poissons Ratio 0.320.32Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 57.0 GPa8270 ksi
Charpy Impact 107 J78.9 ft-lbKeyhole; temper not reported
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000375 ohm-cm
@Temperature 20.0 °C
0.0000375 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity  29.0 W/m-K
@Temperature 20.0 °C
201 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 29.2 W/m-K
@Temperature 100 °C
203 BTU-in/hr-ft²-°F
@Temperature 212 °F
Mill Annealed
 34.1 W/m-K
@Temperature 200 °C
237 BTU-in/hr-ft²-°F
@Temperature 392 °F
Mill Annealed
 38.6 W/m-K
@Temperature 300 °C
268 BTU-in/hr-ft²-°F
@Temperature 572 °F
Mill Annealed
 43.1 W/m-K
@Temperature 400 °C
299 BTU-in/hr-ft²-°F
@Temperature 752 °F
Mill Annealed
 48.1 W/m-K
@Temperature 500 °C
334 BTU-in/hr-ft²-°F
@Temperature 932 °F
Mill Annealed
 53.1 W/m-K
@Temperature 600.0 °C
369 BTU-in/hr-ft²-°F
@Temperature 1112 °F
Mill Annealed
 58.1 W/m-K
@Temperature 700.0 °C
403 BTU-in/hr-ft²-°F
@Temperature 1292 °F
Mill Annealed
Melting Point 1170 - 1240 °C2140 - 2260 °F
Solidus 1170 °C2140 °F
Liquidus 1240 °C2260 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 650 - 825 °C1200 - 1520 °F
Hot-Working Temperature 925 - 1050 °C1700 - 1920 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 70 %70 %
Iron, Fe 0.40 - 0.70 %0.40 - 0.70 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 29 - 33 %29 - 33 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 30%, UNS C71500
Copper nickel 30%, UNS C71500, O61 Temper 19 mm tubing
Copper nickel 30%, UNS C71500, H80 Temper 1 mm strip
Copper nickel 30%, UNS C71500, O61 Temper 1 mm strip
Copper nickel 30%, UNS C71500, H02 Temper 25 mm rod

MC71500b6 / 11749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.