MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources GFF-10 Glass Fiber Felt
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Heat-preservation material of inorganic silicate. By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation.

    Features:
  • Lightness, heat resisting, low thermal capacity and low thermal conductivity, soft and excellent fire-isolation.
  • Anti-heat energy and heat stability.
  • Anti-mildew, anti-insect, and good stretching resistance.
  • Excellent anti-ageing.
  • Excellent sound absorbability, adsorption and filtering.
  • It can be cut, sewn according to requirements and it's also easy to construct.
    Application:
  • This mat is widely used for wrapping material of all kinds of heat source (coal, electricity, oil, and gas) and heat-presentation of central air-conditioning pipelines.
  • It can be used as the materials for heat-isolation and fire-resistance.
  • It can be used as the materials for seal, sound absorption filtering and insulation.
  • Excellent material for heat-conducting, heat-presentation.
  • It can be used as materials for sound isolation, heat insulation and heat-resistance in vehicles, vessels and aircraft.
  • It can also be used for touching fire and all kinds of flue in which the temperature is less than 600ºC.

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness >= 10000 microns>= 394 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 6.00 MPa870 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0280 - 0.0320 W/m-K0.194 - 0.222 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 600 °C1110 °F
 
Descriptive Properties
Weight (g/m²)900-1000
Width (mm)1000-2000±50mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek T-1 Low-Temperature Felt
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Pyrotek LUMIFELT AL20L High Temperature Kevlar® Felt
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications

PBEIJ101 / 90170

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.