MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.

Advantages

  • User-friendly workability
  • Low shrinkage reduces pull-out from joints
  • High strength reduces the risk of erosion of repaired areas and joints
  • Not wetted by molten aluminum

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.820 - 0.880 g/cc0.0296 - 0.0318 lb/in³fired density (compressed)
 1.45 - 1.55 g/cc0.0524 - 0.0560 lb/in³wet density (as supplied)
Loss On Ignition 35 - 40 %35 - 40 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00350 - 0.00400 GPa0.508 - 0.580 ksidried 24 hours @ 120°C
 0.00280 - 0.00350 GPa
@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi
@Treatment Temp. 1380 °F,
Time 24.0 hour
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.160 W/m-K
@Temperature 200 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.200 W/m-K
@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.240 W/m-K
@Temperature 650 °C
1.67 BTU-in/hr-ft²-°F
@Temperature 1200 °F
Maximum Service Temperature, Air 1000 °C1830 °FContinuous
Shrinkage  <= 1.0 %
@Temperature 120 °C,
Time 86400 sec
<= 1.0 %
@Temperature 248 °F,
Time 24.0 hour
 <= 2.0 %
@Temperature 750 °C,
Time 86400 sec
<= 2.0 %
@Temperature 1380 °F,
Time 24.0 hour
fired 24 hours @ 750°C
 <= 2.5 %
@Temperature 1000 °C,
Time 86400 sec
<= 2.5 %
@Temperature 1830 °F,
Time 24.0 hour
fired 24 hours @ 1000°C
 
Descriptive Properties
72 Hour Cup Test 7075 AlloyNo Reaction / Excellent815°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Pyrotek Pyrocast L-30 Moldable Refractory
Pyrotek Dense Fused Silica Pre-Cast Shapes
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement

CPYRO199 / 1916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.